9, The preforms cavities are not injected fully, and melting strips on the preforms.
A, Causes:
   1, Air extraction function is not working well
   2, Injection direction is not straight
B, Solutions:
   1, Increase the air extraction.
   2, Clean the injection mold
   3, Slow down the injection speed
   4, Fix the mold injection holes

10, The preforms uneven thickness
A, Causes:
   1, Molds manufacturing technique is not good
   2, Injection hole is not in right position
   3, Injection pressure is too high
   4, Injection molds core is not in the right place
B, Solutions:
   1, Fix the molds
   2, Increase the material temperature
   3, Reduce the injection pressure
   4, Make good quality molds

http://www.sinobema.com/Difference-between-bottles-of-pure-water?article_id=188
From Sino Beverage Machinery Co., Ltd China
施诺机械设备有限公司中国
sinobema@gmail.com
www.sinobema.com 
www.sinobeveragemachinery.com
WhatsApp: 0086 137 28668423

没有评论:

发表评论

Bottling filling machinery.

Different machines/models for differnet bottles. Email: sinobema@gmail.com WhatsApp: 0086 137 2866 8423 www.sinobema.com Sino Beverage M...