3, Clear/transparent PET preforms change into non-clear preforms

A, Causes:
   1, the temperature for the molds-separating is too high
B, Solutions:
   1, Enhance the cooling water
   2, Increase the cooling time
   3, Change the injection time

4, Fogy shadow appears at any side of the preform.

A, Causes:
   1, Holding pressure is too high.
   2, Bottom injection hole is not in the center.
B, Solutions:
   1, Reduce the pressure
   2, Fix the molds bottom parts.

5, Silver waves or a little-yellow-colors on the PET preforms.

A, Causes:
   1, Plastic decomposition
B, Solutions:
   1, Reduce the dryer temperature, and increase the drying time.
   2, Adjust the injection speed
   3, Reduce the material temperature
   4, Reduce the temperature on the hot nozzles. 

http://www.sinobema.com/Difference-between-bottles-of-pure-water?article_id=185
From Sino Beverage Machinery Co., Ltd China
施诺机械设备有限公司中国
sinobema@gmail.com
www.sinobema.com 
www.sinobeveragemachinery.com
WhatsApp: 0086 137 28668423

没有评论:

发表评论

Labeling machine, for adhesive sticker labels.

More models and more kinds of machinery are available. Email: sinobema@gmail.com WhatsApp: 0086 137 2866 8423 www.sinobema.com Sino Beve...