2019年3月7日星期四

Problems & solutions of PET preforms injection process, Part 7

Problems & solutions of PET preforms injection process, Part 7.


 
16, White or milky color on preforms after adjusting the temperature
A, Causes:
   1, The temperature is too low or too high
B, Solutions:
   1, Change the temperature to a right parameter
   2, Increase the temperature
   3, Make sure the internal and external of the preforms the same

17, Holes on preforms end/bottom
A, Causes:
   1, Temperature for the end/bottom part is too high
   2, Temperature for the preforms body is too low
   3, Raw plastic granules are not good quality
B, Solutions:
   1, Adjust the temperature for the preforms
   2, Get good quality PET granules
   3, Increase the dryer, make sure the PET granules are dried enough.

http://www.sinobema.com/Difference-between-bottles-of-pure-water?article_id=193
From Sino Beverage Machinery Co., Ltd China
施诺机械设备有限公司中国
sinobema@gmail.com
www.sinobema.com 
www.sinobeveragemachinery.com
WhatsApp: 0086 137 28668423

没有评论:

发表评论

PET bottles molding machine.

PET bottles molding machine. Email: sinobema@gmail.com WhatsApp:0086 137 2866 8423 www.sinobema.com