24, PET bottles are easy to be broken by dropping
A, Causes:
   1, Bottle bottom is not stretched properly
   2, PET material damaged in high temperature
B, Solutions:
   1, Change the stretch ratio for the blow molding
   2, Make sure the PET granules are dried enough before injection
   3, Reduce the heating temperature on the injection molding process, or blow molding process

25, Spot or fog inside the PET bottles.
A, Causes:
   1, Dirty air get into the blowing cylinder
   2, High humidity inside the air
B, Solutions:
   1, Check the air filters. If the filters are damaged, try get new filters
   2, Check the air cold dryer, make sure the air is dried enough before getting into the blow molding machine

http://www.sinobema.com/Difference-between-bottles-of-pure-water?article_id=200

From Sino Beverage Machinery Co., Ltd China
施诺机械设备有限公司中国
sinobema@gmail.com
www.sinobema.com 
www.sinobeveragemachinery.com
WhatsApp: 0086 137 28668423

没有评论:

发表评论

What is the air compressore gets very hot after 10 hours working?

  Here are the most common causes, categorized from simplest to most complex: 1. Cooling and Ventilation Issues (Most Common) Poor Ven...