Common problems and solutions for PET preforms injection molding machine, Part 6




Common problems and solutions for PET preforms injection molding machine, Part 6.

13, Bent preforms after getting out of the injection mold.
A, Causes:
   1, Injection hole is not straight, not in the center.
   2, Cooling is not even.
B, Solutions:
   1, Fix the molds.
   2, Reduce the holding pressure
   3, Increase the injection speed
   4, Increase the cooling time
   5, Clean the cooling water tunnel
   6, Increase the pressure and quantity of the cooling water

14, Bent preforms after temperature increasing.
A, Causes:
   1, Preforms core is not straight, not in the middle
   2, Temperature-adjusting hole is not in the core center
   3, Preforms’ density is not even
B, Solutions:
   1, Fix the injection molds
   2, Fix the temperature adjusting parts
   3, Reduce the injection temperature, especially for the bent part of the preforms.

15, White preforms after temperature adjusting
A, Causes:
   1, The temperature for the white part is too high
B, Solutions:
   1, Fix the temperature. Around 80-110 degrees for PET preforms. 

http://www.sinobema.com/Difference-between-bottles-of-pure-water?article_id=191
From Sino Beverage Machinery Co., Ltd China
施诺机械设备有限公司中国
sinobema@gmail.com
www.sinobema.com 

www.sinobeveragemachinery.com
WhatsApp: 0086 137 28668423

没有评论:

发表评论

Bottling filling machinery.

Different machines/models for differnet bottles. Email: sinobema@gmail.com WhatsApp: 0086 137 2866 8423 www.sinobema.com Sino Beverage M...